Zeon Chemicals HyTemp® NS-50 Polyacrylate Curative
Subcategory: Elastomer, TS; Acrylic; Thermoset
Key Words: ACM
Material Notes: HyTemp NS-50 is a 50% active dispersion of sodium stearate in an acrylic elastomer binder. The dispersion functions as a curative with various accelerators in HyTemp 4050, 4060, and AR-70 series elastomers. The dispersion is in the form of purple pellets dusted with clay and free from foreign materials.Standard cure agent for sulfur activated HyTemp 4050, 4060 and AR70 series. (50% active)
|
|
|