Material Notes: HyTemp SC-75 is a 75% active dispersion of a proprietary cure system. The dispersion functions as a cure package in HyTemp 4050 series elastomers. This provides fast property development; excellent shelf stability and good scorch resistance. The dispersion is in the form of green pellets dusted with clay and free from foreign materials.Fast cure package for HyTemp 4050 and 4060 series (75% active)
|
|
|