Zeon Chemicals HyTemp® AR212HR Polyacrylate Curative
Subcategory: Elastomer, TS; Acrylic; Thermoset
Key Words: ACM
Material Notes: HyTemp AR212HR acrylic elastomer contains one or more acrylic esters with a small percentage of a proprietary cure site. Vulcanizates have excellent oil, heat and compression resistance.Acrylic elastomer contains one or more acrylic esters with a small percentage of a proprietary cure site. Vulcanizates have excellent oil, heat and compression resistance.
| Available Properties |
- Mooney Viscosity
- Ash
- Transformation Temperature, Tg
- Heat Loss (%) Max
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|