Zeon Chemicals Hydrin® H1100 Polyepichlorohydrin Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: ECO
Material Notes: Hydrin H1100 is an epichlorohydrin/allyl glycidyl ether copolymer with high oil, fuel and solvent resistance. Compounds using Hydrin H1100 typically exhibit good heat resistance, excellent ozone resistance along with outstanding gas impermeability. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.Hydrin H copolymerized with AGE for sulfur or peroxide vulcanization. Excellent resistance to permeation by gases.
| Available Properties |
- Specific Gravity
- Mooney Viscosity
- Ash
- Transformation Temperature, Tg
- Moisture Content
- AGE Content, %
|
|
|
|