Zeon Chemicals Hydrin® T5010 Polyepichlorohydrin Elastomer
Subcategory: Elastomer, TS; Thermoset
Key Words: ECO
Material Notes: Hydrin T5010 contains ethylene oxide/epichlorohydrin/allyl glycidyl ether. This polymer has high oil, fuel and solvent resistance. Compounds using Hydrin T5010 typically exhibit excellent low and high temperature properties and can be cured using conventional cure systems such as sulfur/sulfur donor or peroxides.This polymer has high oil, fuel and solvent resistance. Compounds using Hydrin T5010 typically exhibit excellent low and high temperature properties and can be cured using conventional cure systems such as sulfur/sulfur donor or peroxides.
| Available Properties |
- Mooney Viscosity
- Ash
- Moisture Content
- AGE Content, %
|
|
|
|