ASTM A572 Steel, grade 45
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Material Notes: Data provided by the manufacturer, Bethlehem Steel Corporation.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|