ASTM A607 Steel, grade 70, cold rolled
Subcategory: Carbon Steel; ASTM Steel; Low Carbon Steel; Metal
Material Notes: Composition includes either 0.005% Nb or 0.01% V.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Shear Modulus
|
|
|
|