AISI Type P4 Mold Steel, air cooled from 955°C, tempered at 425°C
Subcategory: Tool Steel; Special-Purpose Steel; Mold Steel; Metal
Close Analogs: AISI Type P6, AISI Type P20
Key Words: UNS T51604 (Obsolete); ASTM A681(94) P4
Material Notes: Low carbon content and very low hardness help facilitate cold hubbing process. Iron content in composition calcualted as remainder.
| Available Properties |
- Density
- Hardness, Knoop
- Hardness, Rockwell C
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bulk Modulus
- Charpy Impact
|
|
|
|