Asahi Glass Co. ASAHIKLIN AK-225DH Hydrochlorofluorocarbon Solvent
Subcategory: Fluid
Material Notes: AK-225DH was developed as a solvent dewatering and drying system to remove water from the surface of various parts and assemblies. AK-225DH is a mixture of AK-225 and a drying agent to give it rapid water-displacing properties. It is used in specially designed vapor degreaser with all boil sumps. The existing degreaser designed for a mixture of CFC-113 and a drying agent can be used with a few modifications.Information provided by Asahi Glass Company, Inc.
| Available Properties |
- Density
- Viscosity
- Surface Tension
- Heat of Vaporization
- Melting Point
- Boiling Point
- KB Value
- Ozone Depletion Potential (CFC-11 = 1.0)
- Relative Evaporation Rate (ether=100)
- Solubility Parameter
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|