Solvay Solexis Meforex® 124 Ozone-Friendly CFC Replacement
Key Words: CHClFCF3
Material Notes: Formula: CHClFCF3; Name: 1 Chloro 1,2,2,2 Tetrafluoroethane. Replaces CFC 11, 114. Refrigerant blends components for middle temperatures, polystyrene and polyethylene foams. Information provided by Solvay Solexis, Inc.