Solvay Solexis FOMBLIN® Y45 PFPE Lubricant
Subcategory: Fluoropolymer; Polymer; Fluid; Perfluoropolyether (PFPE)
Key Words: Perfluorinated Polyether
Material Notes: FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporative loss; and good viscosity indices. Information provided by Solvay Solexis, Inc.
| Available Properties |
- Density
- Viscosity Measurement
- Kinematic Viscosity at Room Temperature
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Molecular Weight
- Evaporation Loss
- Surface Tension
- Pour Point
- Approximate ISO Grade
- Four Ball Wear Test
- Init. Seiz. Load
- Mean Hertz Load
- Welding Load
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|