Blue River Coatings Undercoat Primer

 

Subcategory: Thermoset; Polymer

Material Notes:
BLUE RIVER COATINGS UNDERCOAT PRIMER is a high quality, single component primer, not requiring any catalyzing agent. Performance obtained is equal or superior to that of two-component, catalyzed epoxy systems. UNDERCOAT PRIMER offers good coverage, excellent durability, and ease of application, as well as being a low VOC and EPA compliant coating.

Enviromental Advantages:BLUE RIVER COATINGS UNDERCOAT PRIMER is a low VOC (Volatile Organic Compound), high performance production coating. It is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent exterior durability
  • Excellent hardness/impact resistance
  • Excellent mar and abrasion resistance
  • Excellent adhesion on plastics and gel coat substrates
  • Solvent resistant
  • Can be applied in a wide variety of temperature and humidity conditions without the use of retarders
  • Distilled water is used for reduction
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • Can be oven baked
  • Wide range of colors
  • Coating will not flash rust on bare metal
  • Shelf life of 1 year
  • Unused paint can be returned to container
  • Non-Flammable
  • Uses

  • Steel
  • Aluminum
  • Fiberglass
  • Concrete
  • Plastics
  • PVC
  • Truck chassis
  • Automobile chassis
  • Trailers
  • Heavy equipment
  • Salt Fog in Harshaw No. 22 cabinet via ASTM B117 procedures with 5% NaCl solution. Evaluation of panels follows ASTM D610, D714, and D1654.

  • 1512 hours
  • Scribed – 1/16” dense #4. Moderate rust rundown OK – moderate rust rundown
  • Unscribed – OK – moderate rust rundown
  • Tested by McWhorter Technologies
  • Information provided by Blue River Coatings

    Available Properties
    • Specific Gravity
    • Density
    • Solids Content
    • Volatile Organic Compounds (VOC) Content
    • pH
    • Impact Test
    • Boiling Point
    • Flash Point
    • Dry Time
    • Shelf Life
    • Adhesion
    • Evporation rate
    • Tape Adhesion
    • Theoretical Coverage
    • Vapor Density
    • Water Submersion
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。