Blue River Coatings Hyfro-Flex Polyurethane Top Coat

 

Subcategory: Polyurethane, TS; Thermoset; Polymer

Material Notes:
BLUE RIVER COATINGS HYDRO-FLEX POLYURETHANE TOPCOAT is a water dispersible polyurethane. When the customer receives HYDRO-FLEX, it is already formed in the container, where as the solvent base type, the polyurethane is formed on the substrate. Therefore, once the paint is applied on the substrate, the film properties of HYDRO-FLEX rival that of other two component catalyzed systems. HYDRO-FLEX offers outstanding coverage, excellent durability, and ease of application as well as being a low VOC and EPA compliant coating.

Enviromental Advantages:BLUE RIVER COATINGS HYDRO-FLEX POLYURETHANE TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent exterior durability
  • Non-photochemically reactive
  • Full gloss-80-85% at 60o glossometer
  • Available in satin to gloss finish
  • Excellent hardness/impact resistance
  • Excellent adhesion, mar, and abrasion resistance
  • Coating will not flash rust on clean dry metals
  • Coatings can be applied in a wide range of temperature and humidity without the use of retarders
  • Linear flexibility is excellent on substrates such as Lexan, vinyl, and fiberglass
  • Water is used for reduction
  • Excellent performance on most plastics
  • Water is used for clean-up
  • Non-Hazardous
  • Air dry or force curing preferred
  • Can be baked dry
  • No discoloration or loss of flexibility when oven baked (250°F for one hour)
  • Wide range of colors
  • Shelf life of 1 year
  • Unused paint can be returned to container
  • Non-Flammable
  • Metallics can be formulated
  • Uses

  • Fiberglass
  • Steel
  • Aluminum
  • Plastic
  • Wood
  • PVC
  • Canvas
  • Information provided by Blue River Coatings

    Available Properties
    • Specific Gravity
    • Density
    • Solids Content
    • Volatile Organic Compounds (VOC) Content
    • Impact Test
    • Taber Abrasion, mg/1000 Cycles
    • Boiling Point
    • Flash Point
    • Dry Time
    • Shelf Life
    • Evporation rate
    • Flexibility
    • Fluid Immersion
    • Pencil Hardness
    • Salt Spray
    • Solvent Resistance
    • Tape Adhesion
    • Theoretical Coverage
    • Vapor Density
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。