Blue River Coatings Hyfro-Flex Polyurethane Top Coat
Subcategory: Polyurethane, TS; Thermoset; Polymer
Material Notes: BLUE RIVER COATINGS HYDRO-FLEX POLYURETHANE TOPCOAT is a water dispersible polyurethane. When the customer receives HYDRO-FLEX, it is already formed in the container, where as the solvent base type, the polyurethane is formed on the substrate. Therefore, once the paint is applied on the substrate, the film properties of HYDRO-FLEX rival that of other two component catalyzed systems. HYDRO-FLEX offers outstanding coverage, excellent durability, and ease of application as well as being a low VOC and EPA compliant coating. Enviromental Advantages:BLUE RIVER COATINGS HYDRO-FLEX POLYURETHANE TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics: Excellent exterior durabilityNon-photochemically reactiveFull gloss-80-85% at 60o glossometerAvailable in satin to gloss finishExcellent hardness/impact resistanceExcellent adhesion, mar, and abrasion resistanceCoating will not flash rust on clean dry metalsCoatings can be applied in a wide range of temperature and humidity without the use of retardersLinear flexibility is excellent on substrates such as Lexan, vinyl, and fiberglass Water is used for reductionExcellent performance on most plasticsWater is used for clean-upNon-HazardousAir dry or force curing preferredCan be baked dryNo discoloration or loss of flexibility when oven baked (250°F for one hour)Wide range of colors Shelf life of 1 yearUnused paint can be returned to containerNon-FlammableMetallics can be formulated Uses FiberglassSteelAluminum PlasticWoodPVCCanvasInformation provided by Blue River Coatings
| Available Properties |
- Specific Gravity
- Density
- Solids Content
- Volatile Organic Compounds (VOC) Content
- Impact Test
- Taber Abrasion, mg/1000 Cycles
- Boiling Point
- Flash Point
- Dry Time
- Shelf Life
- Evporation rate
- Flexibility
- Fluid Immersion
- Pencil Hardness
- Salt Spray
- Solvent Resistance
- Tape Adhesion
- Theoretical Coverage
- Vapor Density
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|