Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat

 

Subcategory: Polyurethane, TS; Thermoset; Polymer

Material Notes:
BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is a water dispersible polyisocyanate coating. HYDRO-GLOSS provides outstanding coverage, excellent durability, and ease of application as well as being a low VOC and EPA compliant coating. HYDRO-GLOSS offers superior adhesion and has film properties that rival most solvent based catalyzed polyurethane systems.

Enviromental Advantages:BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling.

Characteristics:

  • Excellent exterior durability
  • Non-photochemically reactive
  • Full gloss – 92% at 60° glossometer
  • Available in satin to gloss finish
  • Excellent hardness/impact resistance
  • Excellent adhesion, mar, and abrasion resistance
  • Coating will not flash rust on clean, dry metals
  • Coatings can be applied in a wide range of temperature and humidity conditions without the use of retarders
  • Linear flexibility is excellent on substrates such as Lexan, vinyl, and fiberglass
  • Excellent retention of gloss in 1,000 hour QUV weatherometer
  • Water is used for reduction
  • Excellent performance on most plastics
  • Water is used for clean-up
  • Non-Hazardous
  • Wide range of colors
  • Shelf life of 1 year
  • Non-Flammable
  • Metallics can be formulated
  • Uses

  • Steel, Steel Decks
  • Aluminum
  • Vinyl
  • Fiberglass
  • Wood
  • Plastics
  • Canvas
  • Information provided by Blue River Coatings

    Available Properties
    • Specific Gravity
    • Density
    • Solids Content
    • Volatile Organic Compounds (VOC) Content
    • Impact Test
    • Taber Abrasion, mg/1000 Cycles
    • Boiling Point
    • Flash Point
    • Dry Time
    • Shelf Life
    • Evporation rate
    • Flexibility
    • Gloss Retention
    • Pencil Hardness
    • Salt Spray
    • Solvent Resistance
    • Theoretical Coverage
    • Vapor Density
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。