Blue River Coatings Hydro-Gloss 2-Part Polyurethane Top Coat
Subcategory: Polyurethane, TS; Thermoset; Polymer
Material Notes: BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is a water dispersible polyisocyanate coating. HYDRO-GLOSS provides outstanding coverage, excellent durability, and ease of application as well as being a low VOC and EPA compliant coating. HYDRO-GLOSS offers superior adhesion and has film properties that rival most solvent based catalyzed polyurethane systems. Enviromental Advantages:BLUE RIVER COATINGS HYDRO-GLOSS 2-PART POLYURETHANE TOPCOAT is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated; dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics: Excellent exterior durabilityNon-photochemically reactiveFull gloss – 92% at 60° glossometerAvailable in satin to gloss finishExcellent hardness/impact resistanceExcellent adhesion, mar, and abrasion resistanceCoating will not flash rust on clean, dry metalsCoatings can be applied in a wide range of temperature and humidity conditions without the use of retardersLinear flexibility is excellent on substrates such as Lexan, vinyl, and fiberglassExcellent retention of gloss in 1,000 hour QUV weatherometerWater is used for reductionExcellent performance on most plasticsWater is used for clean-upNon-HazardousWide range of colorsShelf life of 1 yearNon-FlammableMetallics can be formulatedUses Steel, Steel DecksAluminumVinylFiberglassWood PlasticsCanvasInformation provided by Blue River Coatings
| Available Properties |
- Specific Gravity
- Density
- Solids Content
- Volatile Organic Compounds (VOC) Content
- Impact Test
- Taber Abrasion, mg/1000 Cycles
- Boiling Point
- Flash Point
- Dry Time
- Shelf Life
- Evporation rate
- Flexibility
- Gloss Retention
- Pencil Hardness
- Salt Spray
- Solvent Resistance
- Theoretical Coverage
- Vapor Density
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|