Blue River Coatings High Performance Acrylic Sanding Sealer
Subcategory: Acrylic; Thermoset; Polymer
Material Notes: BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is a waterbased wood sealer to fill the grain. The product is designed to be a sandable self-sealing topcoat for wood. HIGH PERFORMANCE ACRYLIC SANDING SEALER offers superb application properties, low foam, good adhesion, and excellent sanding properties. HIGH PERFORMANCE ACRYLIC SANDING SEALER dries quickly (eliminating excessive grain raise on wood) and provides excellent sealing properties to help repel water. The product is designed to work in conjunction with Blue River Coatings Wood Stains and Topcoats.Enviromental Advantages:BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is considered non-hazardous by EPA definitions and does not contain lead or chromates. The solid and semi-solid sludge produced in spraying and clean up can be flocculated, dried and sent to a “Class B” landfill. Check with local and state regulations for proper handling. Characteristics: Excellent grain fillerMinimal grain raisingDry to touch in 15 minutes and Dry to sand in 30 minutes at 70°F and 50% humidityCan be applied in a wide variety of temperature and humidity conditionsWater is used for clean-upNon-HazardousShelf life of 1 yearNon-FlammableUses Any wood surface that can be sanded, stained, or selaedInformation provided by Blue River Coatings
| Available Properties |
- Specific Gravity
- Density
- Solids Content
- Volatile Organic Compounds (VOC) Content
- Boiling Point
- Flash Point
- Dry Time
- Shelf Life
- Flexibility
- Pencil Hardness
- Theoretical Coverage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|