Chevron Automatic Transmission Fluid ATF+3®

 

Subcategory: Fluid

Key Words: CPS Number: 238200; MSDS Number: 6801

Material Notes:
General Description

DaimlerChrysler has had their own ATF specifications for many years, but as of 1997, Chrysler owners manuals no longer list DEXRON as an acceptable replacement. ATF+3 is a readily available mineral oil-based ATF that is suitable in any application calling for ATF PLUS® , ATF+2® , or a Type 7176® fluid. Vehicles manufactured after 1999 require ATF+4® , a synthetic-based ATF only available through DaimlerChrysler.

Chevron ATF+3 is specially formulated to optimize performance of Chrysler transmissions and transaxles.

Applications

Chevron ATF+3 Automatic Transmission Fluid is designed for use in all Chrysler automatic transmissions and automatic transaxles where a Mopar ATF PLUS, ATF+2 or ATF+3 fluid is specified.

It is not recommended for use in transmissions spedifying either DEXRON® or MERCON® type fluids

Chevron ATF+3 Automatic Transmission Fluid has been registered with the Chrysler Corperation.

Available Properties
  • API Gravity
  • Brookfield Viscosity
  • Viscosity Measurement
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。