Chevron Journal Bearing Oil

 

Subcategory: Fluid

Key Words: CPS Number: 233803; MSDS Number: 4626

Material Notes:
Features

Chevron Journal Bearing Oil is a high quality, high viscosity index, paraffinic-based lubricant. It incorporates highly effective deposit control antioxidants and rust inhibitors as well as a pour point depressant and viscosity index improver for outstanding year round railroad journal box lubrication.

This product is formulated to exceed the requirements of Association of American Railroads (AAR) Specification M 963 84 for All-Year Journal Box Lubricating Oil.

Chevron Journal Bearing Oil is designed for use in the journal boxes of railcars using plain bearings, not antifriction bearings. The journal box is filled with a waste material which is saturated with Chevron Journal Bearing Oil. The waste, which is against the journal, is heated by friction as the car rolls, causing the oil to slowly feed into the journal bearing. For this reason, a high viscosity index oil is critical. It must have good fluidity at low temperatures and not think excessively at high temperatures.

Chevron Journal Bearing Oil passes:

  • ASTM D 665 Rust Test
  • ASTM D 1748 Corrosion Humidity Cabinet Test

Applications

Chevron Journal Bearing Oil is recommended for the lubrication of journal bearings on the trucks of railcars where a lubricant meeting the requirements of AAR Specification M-963-84 for All-Year Journal box lubricating oil is recommended.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。