Chevron FM Grease EP, NLGI 1
Subcategory: Fluid
Key Words: CPS Number: 230199; MSDS Number: 7882
Material Notes: FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greases EP were developed for the food processing and canning industries.
Chevron FM Greases EP are a blend of a synthetic polyurea complex thickener and food grade white oils (Group II) containing a highly effective rust inhibitor. They are smooth and buttery in texture, and are slightly tacky. All grades contain a specially blended higher viscosity white mineral oil that imparts improved adhesive and stringiness properties to the grease. Applications Chevron FM Greases EP are multipurpose lubricants for all grease lubricated machinery in canneries, beverage bottlers and canners, potato/corn chip processors, candy manufacturers, meat and poultry packers, frozen food processors, and other food producers and processors. They are specifically recommended for critical applications where there is a possibility of the lubricant becoming an incidental or accidental food ingredient. NLGI 1 and 2 are preferred for general plant lubrication including applications such as electric motors and wheeled vehicles where USDA H2 lubricants are often used.
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Weld Load
- Four Ball Wear
- Penetration
- Penetration P(0), 1/10 mm
- Timken Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- Flash Point
- Dropping Point
- Color
- Lincoln Ventmeter, psig at 30 s, at -22°F
- Lincoln Ventmeter, psig at 30 s, at 0°F
- Lincoln Ventmeter, psig at 30 s, at 30°F
- Lincoln Ventmeter, psig at 30 s, at 75°F
- Texture
- Thickener, % / type
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|