Chevron Superla® DCO,

 

Subcategory: Fluid; Lubricant

Key Words: CPS Number: 231076; MSDS Number: 7422

Material Notes:
Features

Chevron Superla DCO is a highly refined food grade white mineral oil that exceeds FDA purity requirements for the dedusting of grains intended for human consumption.

Chevron Superla DCO contains vitamin E, a natural antioxidant, to protect quality during handling and storage.

Applications

Chevron Superla DCO can be used to control dust on animal feeds, chemicals, and fertilizers.

Food grade white mineral oils are widely used for dust control by the grain industry. White oil is applied to the grain just before or during active grain tumbling to prevent dust from escaping the grain stream. For best results, the oil should be applied before the grain enters the storage bin. Only food grade oils that meet the tough standards of the U.S. Food and Drug Administration (FDA) may be used for this application. Chevron Superla DCO does not promote grain rancidity.

Chevron Superla DCO is a field-proven products, fully authorized by the FDA for grain dedusting – at concentrations up to 200 ppm on the grain or rice.

Available Properties
  • API Gravity
  • Saybolt Viscosity at 100°F
  • Kinematic Viscosity at 40°C (104°F)
  • Pour Point
  • Flash Point
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。