Chevron Superla® White Oil, 5
Subcategory: Fluid; Lubricant
Key Words: CPS Number: 231013; MSDS Number: 7292
Material Notes: FeaturesChevron Superla White Oils are colorless, odorless, tasteless mixtures of saturated paraffinic and naphthenic hydrocarbons that span a viscosity range of 50-625 SUS at 100°F. These nearly chemically inert oils are virtually free of nitrogen, sulfur, oxygen and aromatic hydrocarbons. Chevron Superla White Oils contain Vitamin E, a natural antioxidant, to protect quality during handling and storage. They are clear, bright, and free of solids and water. Applications Chevron Superla White Oils find wide application: - where direct food contact may occur
- where prolonged contact with human skin is necessary
- where odor and staining must be minimized
- where outstanding long service under adverse conditions is required
Chevron Superla White Oils must be stored in approved containers to prevent contamination that could jeopardize their food grade status.
| Available Properties |
- Specific Gravity
- API Gravity
- Saybolt Viscosity at 100°F
- Kinematic Viscosity at 40°C (104°F)
- Pour Point
- Flash Point
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|