Chevron ParaLux® Process Oil, 1001R
Subcategory: Fluid
Key Words: CPS Number: 240673; MSDS Number: 7022
Material Notes: FeaturesPARALUX is produced using an all-hydroprocessing route which transforms the molecular structure of undesirable aromatics into highly desirable saturates. This produces a process oil with superior physical and chemical properties : - lower aromatics result in superior color stability.
- Lower volatility improves efficiency.
- Excellent compatibility with rubber polymers reduces processing headaches.
Applications Because PARALUX is produced by all-hydroprocessing, it has performance properties that surpass most conventional paraffinic process oils and approach or surpass many of the performance characteristics of technical white oils. These advantages include: - Exceptionally low aromatic content
- Better color and UV stability than conventional paraffinic or naphthenic oils
- Almost complete resistance to degradation from ultraviolet discoloration
- Lower volatility results in fewer emissions, so less make-up oil is needed and costs are minimized
- Excellent compatibility with rubber polymers which require paraffinic oils. Only all-hydroprocessed oils can deliver all of these advantages
Chevron ParaLux Process Oils are ideal for use in compounding a wide variety of products, including : - Footwear
- Wire and Cable insulation
- Adhesives, sealants and coatings
- Polymer modified asphalts
- Automobile interior moldings
- Automotive under hood parts
- Tires, tire whitewalls, tubes, and inner liners
- Rubber membranes
- Weather Stripping
| Available Properties |
- Specific Gravity
- API Gravity
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Molecular Weight
- Pour Point
- Flash Point
- Refractive Index
- Aniline Point °F
- Aromatics, by HPLC, %
- Carbon Type by n-d-m, % Naphthenic
- Carbon Type by n-d-m, %Aromatic
- Carbon Type by n-d-m, %Paraffinic
- Color
- Saturates, by HPLC, %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|