Chevron ParaMount™ Paraffinic Process Oil, 1001
Subcategory: Fluid
Key Words: CPS Number: 240660; MSDS Number: 8139
Material Notes: FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content. Chevron’s modern all-hydroprocessing technology assures that these oils have very light color and are odorless Chevron ParaMount Paraffinic Process Oils are non-toxic and meet U.S. Food and Drug Administration (FDA) requirement CFR 178.3620( c) for components of non food articles. Applications ParaMount Paraffinic Process Oils function as processing aids or as extender oils in rubber compounding. They are used to: - Reduce the amount of time required for mixing
- Reduce the amount of heat generated in mixing
- Maximizes the dispersion of components
- Extend product volume
- Reduce product cost while maintaining the physical properties of the rubber compound
ParaMount Paraffinic Process Oils are ideal for use in compounding a wide variety of finished rubber products, including:- Footwear
- Agricultural Spray
- Furniture polish
- Textiles
- Wire and Cable insulation
- Adhesives, sealants and coatings
- Polymer modified asphalts
- Asphalt extender
- Automobile interior moldings
- Automotive under hood parts
- Tires, tire whitewalls, tubes, and inner liners
- Insulation
- Gels
- Dielectric Fluids
- Drilling Fluids
- Carpet Underlayment
- Heat transfer fluids
- Foam
- Household products
- Roofing compounds
- Rubber membranes
- Weather Stripping
| Available Properties |
- Specific Gravity
- API Gravity
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flash Point
- Refractive Index
- 21 CFR 178.3620 ( c )
- Aniline Point °F
- Aromatics, by HPLC, %
- Carbon Type by n-d-m, % Naphthenic
- Carbon Type by n-d-m, %Aromatic
- Carbon Type by n-d-m, %Paraffinic
- Color
- Saturates, by HPLC, %
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|