Chevron ParaMount™ Paraffinic Process Oil, 6001

 

Subcategory: Fluid

Key Words: CPS Number: 231018; MSDS Number: 8139

Material Notes:
Features

Chevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.

Chevron’s modern all-hydroprocessing technology assures that these oils have very light color and are odorless

Chevron ParaMount Paraffinic Process Oils are non-toxic and meet U.S. Food and Drug Administration (FDA) requirement CFR 178.3620( c) for components of non food articles.

Applications

ParaMount Paraffinic Process Oils function as processing aids or as extender oils in rubber compounding. They are used to:

  • Reduce the amount of time required for mixing
  • Reduce the amount of heat generated in mixing
  • Maximizes the dispersion of components
  • Extend product volume
  • Reduce product cost while maintaining the physical properties of the rubber compound
ParaMount Paraffinic Process Oils are ideal for use in compounding a wide variety of finished rubber products, including:
  • Footwear
  • Agricultural Spray
  • Furniture polish
  • Textiles
  • Wire and Cable insulation
  • Adhesives, sealants and coatings
  • Polymer modified asphalts
  • Asphalt extender
  • Automobile interior moldings
  • Automotive under hood parts
  • Tires, tire whitewalls, tubes, and inner liners
  • Insulation
  • Gels
  • Dielectric Fluids
  • Drilling Fluids
  • Carpet Underlayment
  • Heat transfer fluids
  • Foam
  • Household products
  • Roofing compounds
  • Rubber membranes
  • Weather Stripping

Available Properties
  • Specific Gravity
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Refractive Index
  • 21 CFR 178.3620 ( c )
  • Aniline Point °F
  • Aromatics, by HPLC, %
  • Carbon Type by n-d-m, % Naphthenic
  • Carbon Type by n-d-m, %Aromatic
  • Carbon Type by n-d-m, %Paraffinic
  • Color
  • Saturates, by HPLC, %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。