Chevron Bright-Cut® Metal Working Fluid, AM

 

Subcategory: Fluid

Key Words: CPS Number: 233944; MSDS Number: 7721

Material Notes:
Features

Chevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.

The unique synthetic antiweld components replace the chlorine and reduce the amount of sulfur and fat typically needed for difficult cutting operations. They are light in color, for improved visibility during machining, and low in odor.

Chevron Bright-Cut Metalworking Fluids formulated with ISOSYN® base stocks provide increased oil life and a safer work environment by increasing the fluid`s flash point, and lowering exposure to aromatics and product vapor, smoking, and misting.

Chevron Bright-Cut Metalworking Fluids:

  • provide excellent cooling and lubrication in a wide range of machining operations
  • prevent welding of chip and tool
  • flush chips away from the work area
  • protect the finished work surfaces, tools and machines against rusting and staining
  • dramatically reduce oil mist in high speed machine tools
The nonstaining oils, Chevron Bright-Cut NL and NM Metalworking Fluids, can be used as dual or tripurpose oils in associated splash, hydraulic or spindle lubrication systems of metalworking machines. Chevron Bright-Cut AM, AH, AXH and AD Metalworking Fluids contain active sulfur and will stain copper and brass.

Applications

Do not use Chevron Bright-Cut Metalworking Fluids in high pressure systems in the vicinity of flames, sparks and hot surfaces. Use only in well ventilated areas. Keep container closed.

The severity of the machining operation and the machinability of the metal are the criteria for selecting the proper cutting oil.

Chevron Bright-Cut NHG Metalworking Fluid

  • Service Classification: Honing/Grinding, Nonstaining
  • A low viscosity cutting oil that is designed for use in light duty machining or honing and grinding operations on ferrous and nonferrous metals, particularly aluminum, magnesium and their alloys. It can also be mixed with other Chevron Bright-Cut and Chevron Elite-Cut® Metalworking Fluids to adjust their compounding to meet the demands of a specific machining operation.

Chevron Bright-Cut NL Metalworking Fluid

  • Service Classification: Light Duty, Nonstaining
  • A light duty product, suitable for general purpose machining of free-machining steels and nonferrous metals. This product is also designed for use in flute grinding operations on difficult tool steels, where it extends wheel life and reduces burning of finished parts found with conventional fluids.

Chevron Bright-Cut NM Metalworking Fluid

  • Service Classification: Medium Duty, Nonstaining
  • The workhorse tri-purpose cutting oil, suitable for automatic screw machine operations on freemachining to intermediate steels, and intermediate to difficult nonferrous metals.

Chevron Bright-Cut AM Metalworking Fluid

  • Service Classification: Medium Duty, Active
  • A versatile, general purpose cutting oil for use with carbon steels and alloy steels. It provides the cooling needed for light-to-moderately severe machining operations and gives excellent tool life and finishes in operations such as tapping, threading, drilling, gear shaving and turning.

Chevron Bright-Cut AH Metalworking Fluid

  • Service Classification: Heavy Duty, Active
  • Provides excellent performance for a wide range of applications. It is suitable for machining tough alloy steels and stainless steels. It is well adapted for broaching, threading, tapping and other difficult operations requiring a heavy duty oil for tool life and finish. This oil may be blended with Chevron Bright-Cut NHG Metalworking Fluid for less severe applications.

Chevron Bright-Cut AXH Metalworking Fluid

  • Service Classification: Extra-Heavy Duty, Active
  • Designed for the most difficult machining operations, such as broaching, tapping and threading on soft stringy steels that tend to tear easily, leaving a poor finish. It is recommended for use with alloy steels, stainless steels, tool and die steels. It is preferred over chlorinated cutting oils for heavy duty machining of difficult nonferrous metals (e.g. titanium, nickel) that are not subject to staining, but may become brittle through the use of chlorinated fluids. This oil may be blended with Chevron Bright-Cut NHG Metalworking Fluid for less severe operations.

Chevron Bright-Cut AD Metalworking Fluid

  • Service Classification: Deep Drilling, Active
  • A low viscosity, heavy duty oil for drilling and reaming deep holes on difficult ferrous and nonferrous metals. It is also recommended for heavy duty machining operations where a lower viscosity cutting oil is preferred. If used with copper or brass, staining will result. However, many brass alloys stain relatively slowly, and in some instances staining can be avoided by washing the oil from the parts shortly after machining.

Available Properties
  • API Gravity
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  • Antimist
  • Synthetic EP, wt%
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。