Chevron Open Gear Lubricants, 250 NC-HT

 

Subcategory: Fluid

Key Words: CPS Number: 250259; MSDS Number: 7088

Material Notes:
Features

Chevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubrication systems.

They provide a high film strength coating on gear teeth to minimize wear.

Chevron Open Gear Lubricants are designed to provide tacky, tenacious lubricant films on open gears operating under severe shock load conditions. Chevron Open Gear Lubricants contain a nonchlorinated diluent that eases the application of these lubricants onto the gears. The diluent then evaporates, leaving a tacky lubricant film on the gear teeth.

They can also be used to lubricate chains, sprockets, wire rope, and cables. When used as a cable coating, the diluent allows the lubricant to penetrate into the core, thus carrying the lubricant into the individual strands and minimizes wear as the cable is run through sheaves or onto a winch drum.

Applications

Chevron Open Gear Lubricants are recommended for all types of open gears, wire ropes, and cables. They can be applied by brush, swab, spray gun, or by automatic lubrication systems.

All grades provide lubrication for mining equipment including:

  • girth and pinion gears on rod and ball mills
  • rack and pinion gears on shovel dipsticks
  • and swing and pinion gears on top of the lower frame of shovels and draglines, which are sometimes served with an automatic lubrication system.
Chevron Open Gear Lubricants meet Bucyrus-Erie and P&H requirements for electric shovels and draglines.

Available Properties
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Timken Test
  • Pour Point
  • Flash Point
  • Color
  • Lincoln Ventmeter, at 400psi, °C
  • Resultant Film
  • Rust Prevention, ASTM D665
  • Texture
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。