Chevron RPM® Gear Oil, SAE 140

 

Subcategory: Fluid

Key Words: CPS Number: 250408; MSDS Number: 6937

Material Notes:
Features

Chevron RPM Gear Oils are straight mineral gear oils.

They are manufactured from specially treated high viscosity index paraffinic base stocks. They contain a metal deactivator to stop such metals as copper from acting as catalysts to promote oil oxidation. They also contain rust, corrosion, and foam inhibitors, plus a pour point depressant to assure fluidity at low temperatures.

Chevron RPM Gear Oils provide long life for gears and bearings in gear cases where the OEM recommends the use of a straight mineral oil.

High viscosity indexes and low pour points assure good film strength and gear wear protection at both high and low temperatures.

Applications

Chevron RPM Gear Oils are recommended for any automotive or industrial equipment where the equipment suppliers recommend the use of a straight mineral oil in SAE viscosity grades 90 (ISO 220) or 140 (ISO 460).

Chevron RPM Gear Oils are also suitable for lubrication of any equipment where copper or bronze is present and susceptible to attack by oils containing sulfurphosphorus compounds.

Chevron RPM Gear Oils meet the requirements of API Service Category GL-1.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Timken Test
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。