Chevron TEGRA® Synthetic Gear Lubricant, ISO 220

 

Subcategory: Fluid

Key Words: CPS Number: 233917; MSDS Number: 6699

Material Notes:
Features

Chevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.

The most advanced formulation has been selected to provide superior load carrying and antiwear properties; protection against rust, corrosion, foaming, and oxidation; and excellent demulsibility. This results in outstanding performance in most types of industrial gearboxes, exemplified by the FZG pass stage results of >12.

These products possess very high shear stability even under heavily loaded, high speed conditions in industrial gears.

The low pour point and very good low temperature fluidity of Chevron Tegra Synthetic Gear Lubricants impart improved lubrication during startup at sub-zero temperatures, while their superior viscositytemperature characteristics provide dependable lubrication at high temperatures.

A unique property of the synthetic base oil is a low traction coefficient, resulting in improved gear efficiency, energy savings, less friction, less wear, and lower operating temperatures compared to conventional mineral oil products.

Due to the very high viscosity index, these products provide a much higher oil viscosity at operating temperature than a mineral oil product of the same ISO grade. This results in increased oil film thickness and better antiwear protection for both bearings and gears. Drain intervals can be extended longer than conventional mineral oil products. That means fewer oil changes, reduced maintenance costs, and less used oil disposal.

Applications

Chevron Tegra Synthetic Gear Lubricants are recommended for all types of enclosed industrial gearboxes, especially those running continuously at temperatures up to 107°C(225°F) or exposed to very cold temperatures as low as -46°C(-50°F), or under severe service conditions, such as heavy loads or low speeds. These products also provide excellent protection for bearings operating under similar conditions. They can be problem-solvers for applications where mineral oil products deteriorate too rapidly or lead to premature failures. Chevron Tegra Synthetic Gear Lubricants meet the requirements of:

  • U.S. Steel 224
  • AGMA 9005 and qualify as AGMA EP gear lubricants
  • major gear manufacturers — Falk, Hedcon, Santasalo, and Sumitomo
Chevron Tegra Synthetic Gear Lubricants meet the requirements of Cincinnati Machine P-35 (ISO 460), P-59 (ISO 320), P-74 (ISO 220), P-77 (ISO 150). Chevron Tegra Synthetic Gear Lubricants meet the requirements (discontinued in 1998) of the U.S. Department of Agriculture (USDA) for use in federally inspected meat and poultry plants as H2 lubricants with no food contact.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Timken Test
  • Pour Point
  • Flash Point
  • FZG Gear Wear Test, Failure Load Stage
  • Rust Prevention, ASTM D665
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。