Chevron Moly Grease EP, NLGI 1

 

Subcategory: Fluid; Lubricant

Key Words: CPS Number: 255659; MSDS Number: 6912

Material Notes:
Features

Chevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybdenum disulfide (moly), EP additive, rust and oxidation inhibitors. They are dark gray/black in color and smooth and buttery in texture.

These products satisfy the demand for high quality moly-type greases with extreme pressure capability in both automotive and industrial applications.

Chevron Moly Greases EP provide excellent performance under extreme pressure, boundary lubrication conditions because of their EP additive and moly content. With a Timken OK Load (ASTM D 2509) of 50 lbs and moly to maintain a low coefficient of friction along sliding surfaces, even under loads exceeding the yield strengths of metals, Chevron Moly Greases EP provide both shock and heavy load protection. Moly provides a lubricity safety factor (staying power) in situations where the grease is depleted and only molybdenum disulfide remains to provide lubrication until more grease is applied.

Chevron Moly Greases EP provide longer-lasting lubrication than conventional greases. Hence, lubrication frequencies can be extended and down time reduced. They are ideal in situations where lubrication is infrequent. The "moly" provides a reserve protection should the lubricant be squeezed from the bearing surface. They have good storage stability, are pumpable at low temperatures, and provide water resistance and rust protection.

Applications

Chevron Moly Greases EP are recommended for use in automotive and industrial equipment where a moly type grease is called for.

Typical applications in automotive equipment are: chassis, bearings, universal joints, fifth wheels, and ball joints in construction equipment such as bulldozers, scrapers, loaders, shovels, etc.

Chevron Moly Greases EP are recommended for use in roller chains, trunions, gears, cables, sheaves, slides, and chassis bearings.

In industrial applications, these greases are recommended for the lubrication of conveyor bearings, sliding and rubbing surfaces, kiln car bearings, etc. They are particularly suited for heavily loaded pivot pins, splined shafts, or other surfaces subjected to sliding, vibration, or oscillation where fretting is encountered.

Chevron Moly Greases EP meet Caterpillar recommendations for greases containing 3% molybdenum disulfide.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Weld Load
  • Penetration
  • Penetration P(0), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Flash Point
  • Dropping Point
  • Color
  • Lincoln Ventmeter, psig at 30 s, at -22°F
  • Lincoln Ventmeter, psig at 30 s, at 0°F
  • Lincoln Ventmeter, psig at 30 s, at 75°F
  • Texture
  • Thickener, % / type
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。