Chevron Moly Grease EP, NLGI 2
Subcategory: Fluid; Lubricant
Key Words: CPS Number: 255660; MSDS Number: 6912
Material Notes: FeaturesChevron Moly Greases EP are general purpose, extreme pressure (EP) greases. They are manufactured using highly refined selected base oils, a lithium-12-hydroxystearate thickener, 3% molybdenum disulfide (moly), EP additive, rust and oxidation inhibitors. They are dark gray/black in color and smooth and buttery in texture. These products satisfy the demand for high quality moly-type greases with extreme pressure capability in both automotive and industrial applications. Chevron Moly Greases EP provide excellent performance under extreme pressure, boundary lubrication conditions because of their EP additive and moly content. With a Timken OK Load (ASTM D 2509) of 50 lbs and moly to maintain a low coefficient of friction along sliding surfaces, even under loads exceeding the yield strengths of metals, Chevron Moly Greases EP provide both shock and heavy load protection. Moly provides a lubricity safety factor (staying power) in situations where the grease is
depleted and only molybdenum disulfide remains to provide lubrication until more grease is applied. Chevron Moly Greases EP provide longer-lasting lubrication than conventional greases. Hence, lubrication frequencies can be extended and down time reduced. They are ideal in situations where lubrication is infrequent. The "moly" provides a reserve protection should the lubricant be squeezed from the bearing surface. They have good storage stability, are pumpable at low temperatures, and provide water resistance and rust protection. Applications Chevron Moly Greases EP are recommended for use in automotive and industrial equipment where a moly type grease is called for. Typical applications in automotive equipment are: chassis, bearings, universal joints, fifth wheels, and ball joints in construction equipment such as bulldozers, scrapers, loaders, shovels, etc. Chevron Moly Greases EP are recommended for use in roller chains, trunions, gears, cables, sheaves, slides, and chassis bearings. In industrial applications, these greases are recommended for the lubrication of conveyor bearings, sliding and rubbing surfaces, kiln car bearings, etc. They are particularly suited for heavily loaded pivot pins, splined shafts, or other surfaces subjected to sliding, vibration, or oscillation where fretting is encountered. Chevron Moly Greases EP meet Caterpillar recommendations for greases containing 3% molybdenum disulfide.
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Weld Load
- Penetration
- Penetration P(0), 1/10 mm
- Timken Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- Flash Point
- Dropping Point
- Color
- Lincoln Ventmeter, psig at 30 s, at -22°F
- Lincoln Ventmeter, psig at 30 s, at 0°F
- Lincoln Ventmeter, psig at 30 s, at 75°F
- Texture
- Thickener, % / type
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|