Chevron RPM® Arctic Grease, NLGI 1
Subcategory: Fluid; Lubricant
Key Words: CPS Number: 259131; MSDS Number: 4727
Material Notes: FeaturesChevron RPM Arctic Grease is a premium quality grease. It is manufactured using a polyurea acetate complex thickener, special low viscosity base oil, and rust and oxidation inhibitors. It is black in color and its texture is smooth and buttery. It is specially formulated for use in automotive and industrial applications where extreme low temperatures are encountered. Chevron RPM Arctic Grease has outstanding low temperature lubrication qualities and provides metal parts with excellent rust and corrosion protection as well as protection from wear. Applications Chevron RPM Arctic Grease is recommended as a premium general purpose automotive and industrial grease where extreme low temperature performance is required. It is also recommended for use in environments with a wide temperature range. It is approved for the NLGI Certification Mark GC LB.
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Penetration
- Penetration P(0), 1/10 mm
- Timken Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- Flash Point
- Dropping Point
- Color
- Lincoln Ventmeter, psig at 30 s, at -22°F
- Lincoln Ventmeter, psig at 30 s, at 0°F
- Lincoln Ventmeter, psig at 30 s, at 30°F
- Lincoln Ventmeter, psig at 30 s, at 75°F
- Texture
- Thickener, % / type
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|