Chevron Rykon® Premium Grease No. 1364,
Subcategory: Fluid; Lubricant
Key Words: CPS Number: 231056; MSDS Number: 7611
Material Notes: FeaturesChevron Rykon Premium Grease No. 1364 contains polyurea thickener in highly refined paraffinic oil, as well as extreme pressure and rust protection additives. Chevron Rykon Premium Grease No. 1364: - is resistant to oil separation during use and storage.
- has excellent high temperature characteristics.
- will not blacken copper or steel when tested for one hour at 150°C (302°F).
Applications Chevron Rykon Premium Grease No. 1364 was formulated specifically for the automotive constant velocity (CV) driveline joints used in front-wheel drive automobiles. It is compatible with the common elastomers used for boots in the joints and can be used in "hot" CV joints up to 177°C (350°F). Chevron Rykon Premium Grease No. 1364 can also be used in other applications requiring a high temperature
grease with extreme pressure additives. Chevron Rykon Premium Grease No. 1364 meets the requirements of GKN specification M-3005 for CV grease.
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Penetration
- Timken Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Dropping Point
- Bearing Rust
- Color
- Texture
- Thickener, % / type
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|