Chevron Sil-X® Grease, SF

 

Subcategory: Fluid; Lubricant

Key Words: CPS Number: 255780; MSDS Number: 6704

Material Notes:
Features

Chevron Sil-X Grease is a silica thickened grease. It is manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.

It is transparent red in color, and has a smooth consistency with distinct stringiness.

Chevron Sil-X Grease provides outstanding lubrication in industrial applications where extremely high temperatures are encountered. The dropping points of Chevron Sil-X Grease exceeds 260°C (500°F). Chevron Sil-X Grease has a very high film strength and performs well under shock load conditions. It minimizes wear and prevents scuffing.

Its high viscosity oil and high viscosity additive characteristics enable this lubricant to seal bearings and resist leakage and washout.

Under high temperature operating conditions, the "no melt" silica keeps the lubricant in place long after conventional multipurpose greases would have melted and run out of bearings.

Chevron Sil-X Grease has an excellent pumpability characteristic.

Applications

Chevron Sil-X Grease is recommended for industrial applications subjected to very high temperatures requiring a lubricant which will not melt.

Typical applications are plain or journal bearings, antifriction bearings, gear cases in kiln cars, conveyors in ceramic and paint baking ovens furnace doors, shafts extending through furnaces, etc.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Penetration
  • Penetration P(0), 1/10 mm
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Flash Point
  • Color
  • Texture
  • Thickener, % / type
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。