FeaturesChevron Thread Sealing Compound is a time-tested aluminum complex grease designed especially for casing and tubing connections in high-pressure oil well service, or wherever unusually severe conditions are encountered.
Chevron Thread Sealing Compound contains copper flake, graphite, and other extreme pressure and antiwear addititves.
Chevron Thread Sealing Compound meets the performance requirements of API Recommended Practice 5A3, First Edition, October1, 1996, “Recommended Practice on Thread Compounds for Casing, Tubing and Line Pipe.”
This grease has superior lubrication to prevent galling in threaded connections during joint makeup, and reduces torque requirements in breaking joints.
Its sealing properties will prevent leakage at temperatures as high as 149°C (300°F), while the quality and quantity of inert fillers prevent leakage of API round thread casing and tubing joints under pressure as high as 10,000 psi.
It has outstanding resistance to water absorption and is readily applied by brush to pipe joints, even in cold weather.
Applications
Chevron Thread Sealing Compound is used for API 8 round thread casings, buttress thread casings, tubing connections, and line pipes. It should not be used in rotary shoulder connections.