Chevron Tool Joint Compound
Subcategory: Fluid; Lubricant
Key Words: CPS Number: 234998; MSDS Number: 6837
Material Notes: FeaturesChevron Tool Joint Compound is an aluminum complex grease designed principally for the lubrication of drill collars, tool joints and pipe threads. It contains copper flake and graphite, fortified with extreme pressure and antiwear additives. Chevron Tool Joint Compound: - provides high antiweld protection and withstands high pressures
- stays on threads under severe torquing action
- protects the shoulders and thread faces of the tool joint against damage from galling or seizure during makeup or disassembly
- provides excellent corrosion, oxidation resistance
- provides good brushability at low temperatures.
Chevron Tool Joint Compound is waterproof and highly resistant to washoff by water or drilling mud.Applications Chevron Tool Joint Compound is the preferred recommendation for the threads and shoulders of rotary shouldered tool joints and the entire drill string in most drilling applications.
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Penetration
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Flash Point
- Dropping Point
- Color
- Texture
- Thickener, % / type
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|