Chevron Cylinder Oil W, ISO 220

 

Subcategory: Fluid

Key Words: CPS Number: 230339; MSDS Number: 7673

Material Notes:
Features

Chevron Cylinder Oils W are designed to meet the needs of emulsifying cylinder oils.

Chevron Cylinder Oils W provide excellent metal wettability. The combination of oil emulsibility and metal wetting characteristics result in lower oil consumption rates and improved oil lubricity in the presence of wet steam or water.

The metal wetting assures an effective lubricant film on the cylinder walls and pistons of steam pumps and engines, and also provides the oiliness properties which are extremely important in lubricating the sliding worm gear surfaces in worm drive gear cases.

Applications

Compressor manufacturers often recommend cylinder oils for compressor cylinder lubrication. The oiliness of Chevron Cylinder Oils W provides a metal wetting characteristic that resists the washing action of water and maintains a tenacious oil film on the surface of the compressor cylinder. The lower viscosity of Chevron Cylinder Oil W ISO 220 makes it suitable for this application in colder climates.

Chevron Cylinder Oil W ISO 460 is recommended for moderate service applications where steam pressures will not exceed 150 psi and temperatures vary between 171°C to 204°C (340°F to 400°F).

Chevron Cylinder Oils W ISO 680 is a higher viscosity lubricant recommended for steam pressures up to 300 psi and temperatures from 218°C to 302°C (425°F to 575°F).

Chevron Cylinder Oils W are ideal choices for worm gears.

Chevron Cylinder Oils W are recommended for use in underground brine pumps at geothermal power generation facilities.

Chevron Cylinder Oils W ISO 220, 460, and 680 meet the requirements of ANSI/AGMA 9005-D94 for AGMA Lubricant Numbers 5, 7 Compounded, 8 Compounded, and 8A Compounded, respectively.

Chevron Cylinder Oils W ISO 460 and ISO 680 are registered with NSF and are acceptable as lubricants where there is no possibility of food contact (H2) in and around food processing areas. The NSF Nonfood Compounds Registration Program is a continuation of the USDA product approval and listing program, which is based on meeting regulatory requirements of appropriate use, ingredient review and labeling verification.

Available Properties
  • API Gravity
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。