Conoco Hydroclear Diamond Class® Turbine Oil 46
Subcategory: Fluid
Material Notes: Description: Conoco Hydroclear Diamond Class Turbine Oil is an extended service life rust- and oxidation-inhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Diamond Class Turbine Oil is specially formulated with proprietary additive chemistry to meet the demands of severe- and long-life turbine service. Hydroclear Diamond Class Turbine Oil has demonstrated successful performance results in severe duty General Electric Frame 7 gas turbines used in co-generation service, easily surpassing historical performance of “premium” turbine oils. It can also be used successfully in steam turbines and other applications which require premium quality rust- and oxidation-inhibited circulating oils. Information provided by ConocoPhillips.
| Available Properties |
- Density
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Oxidative Stability
- ASTM Color
- Dielectric Strength
- Pour Point
- Rotating Bomb Oxidation Test (RBOT)
- Flash Point
- Corrosion, Copper Strip
- Emulsion Characteristics (40-40-0)
- Zinc
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|