Conoco Hydroclear® Rock Drill Oil 46
Subcategory: Fluid
Material Notes: Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill Oil is specially formulated with proprietary additive chemistry and is recommended for use in a variety of pneumatic tool applications which require extreme-pressure properties for protection of equipment under high-load conditions, tackiness for good adhesion to working surfaces, good atomization with low-fogging tendencies and excellent low temperature fluidity. Hydroclear Rock Drill Oil is specifically formulated for use in surface-mining equipment, high- and low-speed drills, jackhammers, paving breakers, vacuum pumps, track-type air drills and other similar applications. Hydroclear Rock Drill Oil can also be used effectively as a saw guide lubricant in lumber mill applications. Hydroclear Rock Drill Oil is available in seven viscosity grades, ISO 32-320, to meet the needs of most applications and operating conditions. Hydroclear Rock Drill Oil exceeds the lubricant specifications for Ingersoll-Rand and Gardner-Denver drilling equipment. Information provided by ConocoPhillips.
| Available Properties |
- Density
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- ASTM Color
- Falex Load Test
- Timken Test
- Pour Point
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|