Conoco Syncon® Synthetic EP Gear Oil 460, AGMA No. 7EP
Subcategory: Fluid; Lubricant
Material Notes: Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is suited for extruder reducers, agitator drives, centrifuge gear boxes and industrial gear drives of spur, helical, herringbone and bevel gear design that require severe-duty, extreme-pressure lubricants. It is also suited for ball, roller and needle antifriction bearings. Syncon Synthetic EP Gear Oil is available in five ISO viscosity grades: 150, 220, 320, 460 and 680. Information provided by ConocoPhillips.
| Available Properties |
- Density
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Load Wear Index
- Four Ball Extreme Pressure, Weld Load
- Four Ball Wear
- Timken Test
- Pour Point
- Flash Point
- ASTM Rust A&B
- Copper Corrosion
- Demulsibility: Emulsion
- Demulsibility: Freewater
- Foam: Sequence I
- Foam: Sequence II
- Foam: Sequence III
- FZG Gear Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|