Conoco SynXPA® H Lubricant HC-450
Subcategory: Fluid; Lubricant
Material Notes: Description: Conoco SynXPA H Lubricant is a premium-quality synthetic-polyolester lubricant that offers exceptional protection for heavily loaded and partially opened open gears, such as those in ball mills, shovels, kilns and draglines. It is also useful for wire ropes, shovel boom sticks and slow moving bearings. It is inherently biodegradable (up to 90 percent biodegradable, as per CEC, OECD testing) and nontoxic (As per acute mammalian toxicity studies.). SynXPA H Lubricant can be applied to the surface through most automatic lubricators or through automated delivery lines and an air assisted sprayer. Pressure-lubrication bins, lines and pumps need not be purged unless they are plugged by residual asphaltic materials. SynXPA H Lubricant meets the performance requirements of the American Gear Manufacturers Association (AGMA) 251.02 Specification for high-viscosity-grade, extreme-pressure gear lubricants. SynXPA H Lubricant offers exceptionally high film strength and film thickness. It spreads out and coats surfaces evenly for better distribution of load. It reduces the gear surface temperatures and minimizes the temperature gradient across the gear face, which typically is associated with slightly misaligned gear sets. Polyolesters have great affinity for metals. As such, SynXPA H Lubricant bonds to gear surfaces and provides exceptional shock loading protection at startups and in situations where the equipment may be idle for extended periods of time. Information provided by ConocoPhillips.
| Available Properties |
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Load Wear Index
- Four Ball Wear
- Penetration
- Timken Test
- Flash Point
- Color
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|