Conoco SynXPA® R&O Oil 32

 

Subcategory: Fluid

Material Notes:
Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acting, single- and multistage reciprocating compressors; in oil-flooded rotary-vane, rotary-lobe and screw compressors; in vacuum pumps that require an oil with low volatility; and in mild-duty industrial gear drives of spur, helical and bevel gear design that require an AGMA 3 or 4 R&O gear lubricant. It is not intended for use in applications which require extreme-pressure (EP) additives, such as spiral-bevel or hypoid gear sets. In ISO 32 and 68, it can be used in mild-duty hydraulic systems where the pump manufacturer specifies a rust- and oxidation-inhibited oil. SynXPA R&O Oil offers superior low-temperature fluidity and excellent high-temperature thermal and oxidative stability up to 400°F. It essentially eliminates the common problems of oil-separator varnishing and plugging, as well as vane sticking. With proper oil analysis, SynXPA R&O Oil can extend oil-drain intervals to 8,000 hours – compared to just 1,000 hours for conventional solvent-refined R&O oils. Do not use SynXPA R&O Oil for systems that require antiwear hydraulic oil. Do not mix it with conventional solvent-refined R&O oils or other synthetic oils.

Information provided by ConocoPhillips.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Penetration
  • Pour Point
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。