Conoco Transformer Oil
Subcategory: Fluid
Material Notes: Description: Conoco Transformer Oil, an insulating oil of very high dielectric strength, is suited for oil-filled transformers in both large substations and small pole-mounted transformers. It is also suited for use in circuit breakers, switches and any other oil-immersed electrical equipment. It meets the requirements of ANSI/ASTM D3487 Type II for inhibited oils. This specification provides uniform functional characteristics for petroleum electrical-insulating oil and is recognized by the Institute of Electrical and Electronic Engineers (IEEE) and other professional societies that deal with insulating materials. It also meets Westinghouse Specification PDS 55822AG and Federal Specification VV-L-530A. Information provided by ConocoPhillips.
| Available Properties |
- Density
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- ASTM Color
- Dielectric Breakdown
- Pour Point
- Rotating Bomb Oxidation Test (RBOT)
- Flash Point
- Acid/Sludge Test
- Aniline Point
- Approved Antioxidant Content
- Corrosive Sulfur
- Gassing Tendency
- Interfacial Tension
- Moisture
- Neutralization No.
- Polychlorinated Biphenyls (PCBs)
- Power Factor
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|