Conoco Transparent Cutting Oil 32
Subcategory: Fluid
Material Notes: Description: Conoco Transparent Cutting Oil is suited for mild to moderate machining that requires a nonstaining fluid to permit view of the work piece. It is recommended for light machining of ferrous and nonferrous metals, such as mild steel, brass, copper, aluminum and magnesium. It also can be used as a hydraulic fluid in machines in which the cutting oil and the hydraulic oil are drawn from a common sump. Information provided by ConocoPhillips.
| Available Properties |
- Density
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- ASTM Color
- Pour Point
- Flash Point
- Chlorine
- Copper Corrosion
- Sulfur
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|