Conoco EP Conolith® Grease NLGI NO. 1

 

Subcategory: Fluid; Lubricant; Organic Soap Gellant

Material Notes:
Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for these bearings when they are subjected to high speeds, moderate temperatures, water and shock loads. It does not contain any tackifiers, which makes it ideal for centralized lubrication systems. EP Conolith Grease is available in several NLGI grades and has been widely accepted in the steel, aluminum and other industries as a general-purpose plant grease. EP Conolith Grease is widely used by the can manufacturing industry because it has, in addition to the required performance characteristics, a light, low-staining, natural color. EP Conolith Grease is manufactured with high-viscosity index paraffinic basestocks and lithium 12-Hydroxy stearate soap stock. It is compounded with an effective extreme-pressure additive and corrosion inhibitors which impart good load-carrying characteristics and good chemical stability.

Information provided by ConocoPhillips.

Available Properties
  • Viscosity Measurement
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F)
  • Kinematic Viscosity at 100°C (212°F)
  • Four Ball Extreme Pressure, Weld Load
  • Four Ball Wear
  • Penetration P(60), 1/10 mm
  • Timken Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Pour Point
  • Dropping Point
  • ASTM Rust A&B
  • Color
  • Low Temperature Mobility
  • Oxidation Stability
  • Shear Stability
  • Soap Type (Thickener)
  • Water Washout
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。