Conoco Milube® Grease 2100T NLGI No. 1
Subcategory: Fluid; Lubricant; Organic Soap Gellant
Material Notes: Description: Conoco Milube Grease is a high-quality, extreme-pressure lithium 12-hydroxy grease with heavy base oil developed for use in heavily loaded industrial heavy-duty bearings characteristic of the steel, aluminum and rubber manufacturing industries. Excellent for use in systems requiring heavy base oil for lubrication where grease pumpability is a concern, such as industrial centralized lube systems. Milube Grease 2100T is identical to Milube 2100 with the addition of an effective tackifier. This helps the grease stay in place under high-temperature or heavily loaded conditions. Information provided by ConocoPhillips.
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Load Wear Index
- Four Ball Extreme Pressure, Weld Load
- Four Ball Wear
- Penetration P(60), 1/10 mm
- Timken Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- Dropping Point
- ASTM Rust A&B
- Color
- Copper Corrosion
- Roll Stability
- Soap Type (Thickener)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|