Conoco Super Lube M EP Grease NLGI No. 2
Subcategory: Fluid; Lubricant; Organic Soap Gellant
Material Notes: Description: Conoco Super Lube M EP Grease is a premium-quality, multipurpose, high-temperature, extreme-pressure (EP) lithium complex grease developed to satisfy the severe requirements of off-road equipment manufactured by Caterpillar, Komatsu-Dresser, J.I. Case, John Deere and others. These include bulldozers, scrapers, off-highway trucks, wheel loaders, pipelayers, skidders, motor graders and soil compactors where the chassis components and wheel bearings are subjected to heavy loading. Super Lube M EP Grease is also recommended for use in automotive and commercial applications such as chassis, wheel bearings, water pump bearings, universal joints, constant velocity joints, brake self-adjusting screws, tractor-trailer fifth wheels and clutch release bearings. Super Lube M EP Grease also can be used in heavily loaded antifriction and plain bearings used in gear boxes and electric motors. These are commonly found in steel, chemical and aluminum manufacturing plants, where the manufacturer specifies a lithium or lithium complex EP corrosion-resistant grease with moly. Information provided by ConocoPhillips.
| Available Properties |
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Load Wear Index
- Four Ball Extreme Pressure, Weld Load
- Four Ball Wear
- Penetration P(60), 1/10 mm
- Timken Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Dropping Point
- ASTM Rust Fresh and Saltwater
- Color
- Molybdenum Disulfide
- Oil Separation
- Oxidation Stability
- Roll Stability
- Soap Type (Thickener)
- Water Washout
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|