Conoco Tacna® 2000 NLGI No. 2
Subcategory: Fluid; Lubricant; Organic Soap Gellant
Material Notes: Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and operated at medium to high ambient temperatures. It is also ideal for use as a fifth wheel grease commonly found on tractor/trailers. The No. 1 grade provides better fluidity and is recommended for lower ambient temperatures. Tacna 2000 is manufactured from high-viscosity index paraffinic base oils and lithium 12-hydroxy stearate soap stock. It is fortified with an adhesive polymer, rust and corrosion inhibitors, and an effective extreme-pressure additive, which results in an exceptionally stable grease that resists separation under heavy loads. It is also extremely resistant to water washing, as evidenced by its excellent water-washout and spray-off characteristics. Tacna 2000 contains an effective polymer which prevents oil bleeding while providing an exceptional level of protection under shock loading conditions. Information provided by ConocoPhillips.
| Available Properties |
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Weld Load
- Four Ball Wear
- Penetration
- Penetration P(60), 1/10 mm
- Timken Test
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Pour Point
- Dropping Point
- ASTM Rust Test (A & B)
- Color
- Copper Corrosion
- Low Temperature Mobility
- Oxidation Stability
- Roll Stability
- Soap Type (Thickener)
- Water Spray Off
- Water Washout
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|