Conoco ANDEROL® 6680 Synthetic Food Grade Gear Fluid
Subcategory: Fluid; Lubricant
Close Analogs: Anderol® is a registered trademark of The Anderol Company.
Material Notes: Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental food contact can occur. ANDEROL 6000 Series Fluids are made for use in gear sets, bearings, circulating oil systems and chain applications. The heavier viscosity grades provide excellent service in worm gear units. ANDEROL food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. ANDEROL food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.” Information provided by ConocoPhillips.
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Four Ball Extreme Pressure, Weld Load
- Four Ball Wear
- Pour Point
- Flash Point
- Copper Corrosion
- Rust Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|