Conoco ANDEROL® HTC PG 150 Chain & Way Fluid, Synthetic Polyglycol Food Grade Fluid ISO 150
Subcategory: Fluid; Lubricant; Polyglycol
Close Analogs: Anderol® is a registered trademark of The Anderol Company.
Material Notes: Description: ANDEROL HTC PG 150 Chain & Way Fluid is a high-temperature chain and way fluid formulated with PTFE to provide lubrication when the PAG is evaporated at high-temperature operation. HTC PG 150 Fluid meets the former H-1 approval requirements of the USDA where incidental food contact can occur. HTC PG 150 Fluid is recommended for use in chains and ways, including high water applications. It also can be used in low-speed gear sets, bearings and circulation systems. ANDEROL food grade lubricants are approved, recommended and field tested by many OEMs in the food processing, baking, bottling, canning, meat processing and pharmaceutical industries. ANDEROL food grade lubricants are listed by NSF International under “USDA Regulations, Proprietary Substances and Nonfood Compounds.” Information provided by ConocoPhillips.
| Available Properties |
- Specific Gravity
- Saybolt Viscosity at 100°F
- Saybolt Viscosity at 210°F
- Kinematic Viscosity at 40°C (104°F)
- Kinematic Viscosity at 100°C (212°F)
- Pour Point
- Flash Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|